title: ASTM A182 F22 合金鋼法蘭 | 2.25Cr-1Mo 鉻鉬鋼 - Gangyou Steel
description: 符合 ASME B16.5/B16.47 標準的 2.25Cr-1Mo (UNS K21590) 材質的 ASTM A182 F22 法蘭，1 級和 3 級。請確認尺寸、等級和密封面以取得報價。
image: https://zh-hant.pipemanufactory.com/uploads/images/astm-a182-f347-flange-4.webp
---

![ASTM A182 F22 合金鋼法蘭](/uploads/images/astm-a182-f347-flange-4.webp)

# ASTM A182 F22 合金鋼法蘭

ASTM A182 F22 合金鋼法蘭，鍛造成 2.25Cr-1Mo (UNS K21590)，用於高溫蒸汽和氫氣環境，按 ASME B16.5 和 B16.47 分為 1 級和 3 級。請確認尺寸、級別和法蘭面以便報價。

**材料**

ASTM A182 F22 (2.25Cr-1Mo), UNS K21590, W.Nr. 1.7380

**級別**

3 級標準化並調質；1 級可按要求退火

**法蘭類型**

焊頸、套焊、盲板、承插焊、螺紋、重疊接頭、長焊頸、孔板

**尺寸範圍**

NPS 1/2-24 對應 ASME B16.5；NPS 26-60 對應 ASME B16.47 系列 A/B

**壓力等級**

150-2500等級（ASME B16.5，2500等級至NPS 12）；按系列的B16.47等級

**密封面**

凸面法蘭 (RF)、環型接頭法蘭 (RTJ)、平面法蘭 (FF)

[發送詢價](/inquiry?products=1543) [WhatsApp](https://wa.me/8615875546993)

## 產品說明

ASTM A182 F22 是一種鍛造 2.25Cr-1Mo（2¼ 鉻、1 鉬）低合金鋼級，用於高溫高壓工況下的管法蘭、鍛造管件及閥門零件。依此鋼種訂購的法蘭標示為 UNS K21590 及歐洲標號 W.Nr. 1.7380 (10CrMo9-10)；ASME SA-182 F22 則是該材料在鍋爐與壓力容器規範中的對應規格。

該鋼種通常以 **3 級、正火及回火處理** 狀態供應，此為管路及壓力部件的預設狀態。若需較低硬度或用於成形應用，可應要求提供 Class 1，退火處理 規格。法蘭尺寸、鑽孔規格及壓力等級並非由 A182 規範所規定，而是依據 ASME B16.5、ASME B16.47 或訂單中指定的圖面而定。

F22 在蠕變強度方面優於 F11（1.25Cr-0.5Mo），在抗高溫氫侵蝕能力方面則優於碳鋼，因此它是傳統發電廠主蒸汽管線和熱再熱管線，以及氫處理器、加氫裂解器與合成迴路法蘭接頭的標準選擇。此為低合金鋼，而非不鏽鋼，且並非因抗水腐蝕性而選用。請於詢價時確認適用規範、等級、表面處理及熱處理要求。

## 化學成分與產品形式

下表列出 F22 級別的 ASTM A182 / ASME SA-182 熔煉分析限值。此範圍同樣適用於 1 級和 3 級，兩者僅在熱處理及由此衍生的驗收值上有所不同。

| 元素 | ASTM A182 F22 (%) |
| --- | --- |
| 碳，C | 0.05 – 0.15 |
| 錳，Mn | 0.30 – 0.60 |
| 磷，P | 最大 0.040 |
| 硫，S | 最大 0.040 |
| 矽，Si | 最大 0.50 |
| 鉻，Cr | 2.00 – 2.50 |
| 鉬，Mo | 0.87 – 1.13 |
| 鐵，Fe | 餘量 |

在詢價階段有兩點需特別留意。ASTM A336 F22 規範涵蓋鍋爐及壓力容器鍛件所用的相同合金，但將磷與硫的含量分別限制在最高 0.025%，並要求進行夏比 V 型缺口衝擊試驗， 因此應明確指明適用規範，而非自行假設。此外，**F22V**（2.25Cr-1Mo-0.25V）為獨立鋼級，專為厚壁氫處理設備而刻意添加釩；其不可與普通 F22 互換使用。

## F22 第 1 級與第 3 級的機械性能

F22 提供兩種熱處理狀態，且必須在詢價時明確標示等級，因為其驗收值有所不同。下表為 ASTM A182 規範中室溫下的要求值。

| 性質 | 第 1 級（退火） | 第 3 級（正火及回火） |
| --- | --- | --- |
| 抗拉強度，最小值 | 415 MPa (60 ksi) | 515 MPa (75 ksi) |
| 屈服強度，最小值 | 205 MPa (30 ksi) | 310 MPa (45 ksi) |
| 50 mm 伸長率，最小 | 20% | 20% |
| 截面積減少率，最小 | 35% | 30% |
| 硬度 | 最大 170 HBW | 156 – 207 HBW |
| 典型用途 | 焊接堆焊母材、成形 | 管路及壓力部件（預設） |

ASTM A182 僅針對 F22 列出 1 級與 3 級規格。2 級規格僅適用於 F11 及 F12，不適用於 F22；若詢價時引用「F22 2 級」，應在放行鍛件前重新說明。根據 A182 規範，衝擊試驗並非強制性要求；若低溫韌性至關重要，則應在訂單中列為補充要求。針對酸性介質服務，NACE MR0175 / ISO 15156 規定此等級的硬度上限為 22 HRC，此限制必須納入熱處理週期中，而非事後進行檢測。

在 450 °C 以上，設計應以蠕變為考量，而非室溫屈服強度。允許應力應參照 ASME BPVC 第 II 卷 D 部分，而非上文的驗收表。

## 法蘭類型、尺寸與壓力等級

F22 可鍛造為 B16.5 標準中的所有法蘭類型。下表彙總了尺寸標準所公布的內容；實際所需的法蘭類型、尺寸與等級，則由專案的管線等級決定。

| 項目 | 適用範圍 |
| --- | --- |
| 材料標準 | ASTM A182 / ASME SA182，F22 級 (UNS K21590) |
| 法蘭類型 | 焊接頸式、套接式、盲板式、承插焊式、螺紋式、搭接式、長焊接頸式、孔板式、縮徑式、眼鏡式盲板 |
| 尺寸，ASME B16.5 | NPS 1/2 至 NPS 24 (DN 15 至 DN 600) |
| 尺寸，ASME B16.47 | NPS 26 至 NPS 60（DN 650 至 DN 1500），A 系列與 B 系列 |
| 壓力等級 | ASME B16.5 150、300、400、600、900、1500、2500 級；ASME B16.47 各系列對應等級 |
| 端面型式 | 凸面（RF）、環形接頭（RTJ）、平面（FF） |
| 焊接端面處理 | 對接焊端面符合 ASME B16.25 規範；管孔直徑與管徑規格相符 |
| 孔板法蘭 | ASME B16.36，採用 B16.5 尺寸 |
| 認證 | EN 10204 3.1 或 3.2 廠方測試證書；可應要求提供材料成分分析（PMI）及硬度檢測報告 |

B16.5 與 B16.47 屬於各自獨立的尺寸系列，而非同一份型錄；相同尺寸與等級的 A 系列與 B 系列通常無法相互螺栓連接——必須明確標示所屬系列。名義尺寸相符亦不能證明可相互配合：外徑、螺栓圓、孔數與孔徑、厚度、法蘭芯、內徑及端面均須與配對組件一致。

## 壓力等級的實際含義

常見將「Class 2500」解讀為「2500 psi」。該等級數值為無量綱的評級指標，並非壓力值。根據 ASME B16.5 標準，各級別的最大允許非衝擊工作壓力需參照法蘭材料組的壓力-溫度表查閱，且該數值會隨設計溫度升高而降低。F22 鍛件列於 B16.5 材料組 1.10 中，與 A217 WC9 鑄件及 A387 22 級鋼板同屬此組，該組的評級表適用範圍延伸至 1200 °F (650 °C)，其中 Class 150 的上限為 1000 ° F（538 °C）。

由此衍生出兩項後果。在 ASME B16.5 標準中，Class 2500 僅公布至 NPS 12 為止——較大尺寸則轉由 ASME B16.47 規範。此外，接合處的極限壓力可能由相連的管線、閥門、墊片或螺栓連接決定，而非由法蘭本身決定。請指定等級（而非 psi 數值），並參閱標準現行版本中關於設計溫度與壓制溫度的評定值。

## F22 與 F11、F91 及 F22V 的比較

F22 是鉻鉬鋼系列中的其中一級。下表展示其在該系列中的定位；此表並非允許應力的來源，允許應力應參照設計規範。

| 鍛造等級 | 名義成分 | 適用範圍 |
| --- | --- | --- |
| F11 | 1.25Cr-0.5Mo | 約 593 °C 以下的熱工程及蒸汽管線，此處無需 F22 的額外蠕變強度 |
| F22 | 2.25Cr-1Mo | 主蒸汽管線、熱再熱管線、氫處理及合成迴路 —— 本頁所列鋼級 |
| F22V | 2.25Cr-1Mo-0.25V | 厚壁加氫處理反應器及封閉鍛件 |
| F5 | 5Cr-0.5Mo | 存在硫化物腐蝕的高鉻煉油應用 |
| F9 | 9Cr-1Mo | 煉油廠高溫侵蝕工況 |
| F91 | 9Cr-1Mo-V-Nb | 超臨界蒸汽；具有較高的蠕變強度，但焊接與熱處理要求更嚴格 |

比較已發佈的表格時，請留意 UNS 標號。第三方彙編資料常會將相同化學成分的管材（A335 P 系列）與鍛件（A182 F 系列）編號混為一談，且有多份網路表格會將管材編號與鍛件等級對應。若 UNS 標號在合約中至關重要，請以採購訂單上指定的版本為準，而非參考頁面上的資訊。

## 高溫蒸汽、氫氣工況及腐蝕極限

有兩種工況決定了 F22 的規格，而關於該等級的一項常見誤解值得在開頭就予以糾正。

**高溫蒸汽。** 由於鉬含量達全百分比，F22 的蠕變強度明顯高於 F11。在傳統化石燃料發電廠中，它是主蒸汽管、熱再熱集管、熱鍋爐連接管及渦輪引管之標準材料，適用溫度範圍最高可達 550–595 °C；此為選材範圍，而非額定值。在 450 °C 以上，設計主要由蠕變強度而非屈服強度決定，因此允許應力應參照 ASME BPVC 第 II 卷 D 部分或適用之設計規範，而非本頁所列之驗收值。

**耐高溫氫侵蝕性。** 在高溫及高氫分壓條件下，鋼中的碳會與氫反應生成甲烷，由於甲烷無法從金屬中擴散出去，將導致內部龜裂及起泡。F22 中 2.25% 的鉻含量可鎖住碳元素，並提高此現象構成風險所需的溫度與氫分壓。允許的組合由 API 941 中的 Nelson 曲線標示，其中 2.25Cr-1Mo 的位置高於碳鋼及 1.25Cr-0.5Mo。正因如此，氫處理器與加氫裂解反應器迴路、氨與甲醇合成迴路，以及氫氣回收壓縮機管路，通常會將 F22 法蘭與 A335 P22 管材及 A234 WP22 管件指定為配套組合。

**F22 並非什麼材料。**F22 的鉻含量為 2.25%，屬於低合金鋼——遠低於形成鈍化表面膜所需的 10.5% 鉻含量。它並非不鏽鋼，對水介質腐蝕毫無實質抵抗力：在環境濕式工況下，其生鏽程度與碳鋼無異。其合金成分旨在提升高溫下的蠕變強度和抗氫性能，而非抗腐蝕性。若需對抗濕式腐蝕，應選用 300 系列或雙相不鏽鋼等級；針對高溫硫化物煉油流體，則應選用鉻含量更高的 F5 和 F9 等級。

## 熱處理、焊接與焊後熱處理

F22 確實具有空氣淬火特性：焊縫的熱影響區在靜止空氣中會自行淬硬，因此製造過程必須事先規劃，而非即興應變。每件 F22 鍛件均經過熱處理，法蘭即以該狀態供應。典型製造要求摘要如下。

| 項目 | 典型要求 |
| --- | --- |
| 鍛件的熱處理 | 正火與回火，或淬火與回火； 至少在 675 °C (1250 °F) 進行 3 級回火 |
| 焊接前預熱 | 通常為 200–300 °C (392–572 °F) |
| 耗材 | 適用於 2.25Cr-1Mo 的焊材：E9018-B3（SMAW）、ER90S-B3（GTAW / GMAW） |
| 焊後熱處理 | 2.25Cr 級別必須進行 — 通常為 690–750 °C (1275–1380 °F) |
| 焊後熱處理溫度限制 | 必須低於母材鍛件所施行的回火溫度 |
| 實務要點 | 低氫耗材、受控的道間溫度、熔爐編號的完整可追溯性 |

其中兩項應從一開始就列入採購訂單。根據 ASME B31.1 及 B31.3 規範，2.25Cr 級材料在幾乎所有實際厚度下均需進行焊後熱處理，因此必須納入施工規範，而非事後追加。此外，焊後熱處理（PWHT）的溫度必須低於母材鍛件所使用的回火溫度：即使法蘭本身在離開鍛造廠時符合規格，接頭處的過度回火仍會破壞法蘭的認證機械性能。

若管線等級允許使用套接法蘭，其成本較低且安裝更為簡便；但在蠕變範圍及週期性工況下，通常僅限採用焊頸式設計，因其全熔透對接焊可進行射線檢測，且抗熱疲勞性能優於角焊縫。

針對厚壁或長壽命高溫工況，訂單中可能還會包含回火脆化控制措施——包括焊縫金屬的 J 因子限值與 Bruscato X-bar 限值——並需進行階梯式冷卻及夏比衝擊試驗。這些屬於補充要求：它們不屬於 A182 基礎標準的一部分，必須在詢價時明確說明。

## ASTM A182 F22 法蘭的應用

典型應用包括：

- 傳統及 HRSG 發電廠中的主蒸汽與熱再熱集管、熱鍋爐連接件及渦輪引管。
- 加氫處理器、加氫裂解器及重整反應器迴路，以及氫氣回收壓縮機管路，此處法蘭接頭必須符合 API 941 奈爾森曲線規範。
- 氨與甲醇合成迴路，以及高壓分離器與熱閃蒸鼓的接管連接處。
- 煉油廠與石化廠的高溫工藝管路，通常作為搭配 A335 P22 管材及 A234 WP22 管件的 2.25Cr-1Mo 系統的一部分。

設計溫度、氫氣分壓以及任何含硫工況要求，是決定是否僅需普通 F22 鋼級，抑或需採用 F22V 或 9Cr 鋼級的三大考量因素。在確定鋼級與熱處理方式前，請先確認這些參數。

## 訂購資訊

如需報價 ASTM A182 F22 法蘭，需提供以下資訊：

- **鋼級與等級** —— ASTM A182 F22 1 級或 3 級。3 級為預設選項；F22 並無 2 級規格。
- **法蘭類型與端面** —— 焊接頸、套接式、盲板、承插焊、螺紋、搭接式、長焊接頸或孔口；RF、RTJ 或 FF。
- **尺寸與壓力等級** —— 公稱尺寸及對應的尺寸標準：ASME B16.5、ASME B16.47 A 系列或 B 系列、ASME B16.36，或相關圖紙。
- **內徑或管壁厚度等級** —— 焊接頸部及長焊接頸部類型必須指定此項，以確保內徑與配對管件相符。
- **熱處理及焊後熱處理（PWHT）說明**，以及任何硬度或 NACE MR0175 / ISO 15156 要求。
- **數量、標記、目的地及文件** —— 視情況提供 EN 10204 3.1 或 3.2 廠方測試證書、材料成分分析（PMI）、硬度檢測報告及第三方檢驗報告。

請在詢價單中註明所需的交貨日期，以便在報價時確認交期。法蘭上標有等級、尺寸、等級類別及爐號，以確保可追溯性。

相關頁面：完整的 [法蘭產品系列](/products/pipe-fittings)，包含其他材料等級與法蘭類型， [合金鋼管](/products/steel-pipe/alloy-steel-pipe)系列（適用於匹配的 A335 P22 產品線），以及 [ASTM A182 F347 法蘭](/products/pipe-fittings/stainless-steel-flange/astm-a182-f347-flange-stabilized-347)頁面（另一種鍛造 A182 等級）。

## 關於 ASTM A182 F22 法蘭的常見問題

### F22 與 2.25Cr-1Mo 及 UNS K21590 是同一種材質嗎？

是的。ASTM A182 F22、2.25Cr-1Mo（2¼Cr-1Mo）、UNS K21590 以及 W.Nr. 1.7380 / 10CrMo9-10 均指同一種鍛造低合金鋼，而 ASME SA-182 F22 則是與 ASTM 標示相對應的規範代號。與其配套的管件規格為 A335 P22 及 A234 WP22 —— 化學成分相同，僅產品形式不同。

### F22 第 1 級與第 3 級有何區別？

熱處理及其所產生的強度。第 1 級經過退火處理，最低抗拉強度為 415 MPa（60 ksi），最低屈服強度為 205 MPa（30 ksi），硬度上限為 170 HBW。第 3 級經正火及回火處理，其最低抗拉強度為 515 MPa（75 ksi），最低屈服強度為 310 MPa（45 ksi），硬度範圍為 156–207 HBW，用以證明其熱處理狀態。第 3 級是管線及受壓部件的���設規格；第 1 級則適用於較低硬度或成形應用，例如焊接堆焊的母材。

### F22 有第 2 級嗎？

沒有。ASTM A182 僅針對 F22 公布第 1 級和第 3 級；第 2 級僅存在於 F11 和 F12。採購方常會沿用 F11 的習慣。若詢價單中標註「F22 2 級」，則在放行鍛件前應重新明確該等級。

### 2500 級是否等同於 2500 psi？

不。等級編號是一種無量綱的評級指標。2500 級法蘭的最大允許工作壓力取決於其材料組別及設計溫度，並可從 ASME B16.5 的壓力－溫度表中查閱；F22 鍛件屬於材料組別 1.10。在 B16.5 標準中，Class 2500 僅公布至 NPS 12 為止。請指定等級而非 psi 數值，並參照標準現行版本的評級值。

### ASTM A182 F22 是否屬於不鏽鋼，且具有抗腐蝕性？

不是。F22 的鉻含量為 2.25%，屬於低合金鋼，遠低於形成鈍化表面膜所需的 10.5% 鉻含量。它在潮濕環境中會像碳鋼一樣生鏽，因此不應指定用於抗水腐蝕的場合。其合金化設計旨在提升蠕變強度及抵抗高溫氫侵蝕。若需應對濕腐蝕，應選用 300 系列或雙相不鏽鋼等級。

### F22 是否需要進行焊後熱處理？

是的。F22 屬於空氣淬硬型鋼材，因此焊縫的熱影響區會自行淬硬；此外，ASME B31.1 和 B31.3 規範要求，對於 2.25Cr 級鋼材，在幾乎所有實際厚度下均須進行焊後熱處理—— 通常為 690–750 °C (1275–1380 °F)。焊後熱處理（PWHT）的溫度必須低於母材鍛件所施加的回火溫度。請將預熱、搭配 2.25Cr-1Mo 焊材以及焊後熱處理一併納入製造時程中。

### 報價需要哪些資訊？

鋼種與等級；法蘭類型與端面處理；尺寸與壓力等級，連同尺寸標準；焊接頸型法蘭的內徑或管徑規格；熱處理與焊後熱處理（PWHT）說明；數量與目的地；以及所需的認證——EN 10204 3.1 或 3.2、材料成分分析（PMI）、硬度檢測或第三方檢驗。

## 您可能還喜歡

[看更多](/products)

![ASTM A105 碳鋼法蘭](/uploads/images/a105-carbon-steel-flange-1.webp)

### [ASTM A105 碳鋼法蘭](/products/pipe-fittings/carbon-steel-flange/astm-a105-carbon-steel-flange)

**鍛造規格**

ASTM A105/A105M（現行版本 A105/A105M-26）

**產品形式**

鍛造碳鋼法蘭，不是板材切割

![ASME B16.5 ASTM A694 F60級法蘭](/uploads/images/asme-b165-astm694-grf60-flange-1.webp)

### [ASME B16.5 ASTM A694 F60級法蘭](/products/pipe-fittings/carbon-steel-flange/asme-b16-5-astm-a694-grade-f60-flange)

**材料標準**

ASTM A694 / ASME SA694，F60 級高強度碳鋼鍛件

**尺寸**

ASME B16.5 (公稱直徑 1/2-24)；ASME B16.47 A/B 系列 (公稱直徑 26-60)；MSS SP44

![ASTM A350 LF2 低溫碳鋼法蘭](/uploads/images/astm-a350-lf2-flange-for-low-temperature-2.webp)

### [ASTM A350 LF2 低溫碳鋼法蘭](/products/pipe-fittings/carbon-steel-flange/astm-a350-lf2-low-temperature-carbon-steel-flange)

**材料**

ASTM A350/A350M 等級 LF2（ASME SA350）、UNS K03011 鍛造碳鋼

**材料類別**

購買訂單上寫的是第 1 類還是第 2 類

![碳鋼鬆套法蘭（Lap Joint）](/uploads/images/s31803-blind-flange-3.webp)

### [碳鋼鬆套法蘭（Lap Joint）](/products/pipe-fittings/carbon-steel-flange/carbon-steel-lap-joint-flange)

**背襯環材質**

ASTM A105 / ASME SA-105 鍛造碳鋼 (UNS K03504); ASME B16.5 材料組 1.1

**翻邊短節（Stub End）**

ASME B16.9 單面接合短端或長短款式；ASTM A234 WPB 碳鋼管用

```json
{"@context":"https://schema.org","@graph":[{"@type":"Organization","@id":"https://pipemanufactory.com/#organization","name":"Gangyou Steel Manufacture Company","alternateName":"Gangyou Steel","url":"https://pipemanufactory.com","logo":"https://pipemanufactory.com/uploads/images/ecfa6bb3-faec-48b0-8daa-81c94219bdaa.png","description":"Gangyou Steel supplies steel pipe, plate, coil, flanges, pipe fittings, fasteners, structural sections, round bar and industrial valves in carbon, stainless and alloy steel, from Foshan, China.","telephone":"+86-15875546993","email":"info@pipemanufactory.com","address":{"@type":"PostalAddress","streetAddress":"Gangtieshijie D7Qu 401 Jiagongqu er Road","addressLocality":"Foshan","addressRegion":"Guangdong","postalCode":"528000","addressCountry":"CN"},"contactPoint":{"@type":"ContactPoint","telephone":"+86-15875546993","email":"info@pipemanufactory.com","contactType":"customer service","availableLanguage":["en","es","de","fr","it","nl","pt","th","ko","vi","ja","id","ru","tr","zh-Hant","ar","no","hmn"]},"sameAs":["https://www.facebook.com/jerry.he.7731","https://www.instagram.com/jerry.he.7731"],"knowsAbout":["https://en.wikipedia.org/wiki/Steel","https://en.wikipedia.org/wiki/Stainless_steel","https://en.wikipedia.org/wiki/Carbon_steel","https://en.wikipedia.org/wiki/Alloy_steel","https://en.wikipedia.org/wiki/Duplex_stainless_steel","https://en.wikipedia.org/wiki/Pipe_(fluid_conveyance)","https://en.wikipedia.org/wiki/Piping_and_plumbing_fitting","https://en.wikipedia.org/wiki/Flange","https://en.wikipedia.org/wiki/Fastener","https://en.wikipedia.org/wiki/Valve","https://en.wikipedia.org/wiki/Structural_steel","https://en.wikipedia.org/wiki/Sheet_metal","https://en.wikipedia.org/wiki/Galvanization"],"hasCertification":[{"@type":"Certification","name":"PED 2014/68/EU 指令","issuedBy":{"@type":"Organization","name":"TUV Rheinland"},"validFrom":"2024-03-29"},{"@type":"Certification","name":"ASME U-Stamp 認證","issuedBy":{"@type":"Organization","name":"The American Society of Mechanical Engineers"},"validFrom":"2023-11-14"},{"@type":"Certification","name":"NORSOK M-650 資格認證","issuedBy":{"@type":"Organization","name":"DNV GL"},"validFrom":"2024-07-07"},{"@type":"Certification","name":"ISO 3834-2 焊接認證","issuedBy":{"@type":"Organization","name":"TUV Nord"},"validFrom":"2024-08-11"},{"@type":"Certification","name":"Lloyd Register 類型批准","issuedBy":{"@type":"Organization","name":"Lloyd Register"},"validFrom":"2024-05-04"},{"@type":"Certification","name":"中國 CCC 認證","issuedBy":{"@type":"Organization","name":"CNCA"},"validFrom":"2024-08-31"},{"@type":"Certification","name":"ABS 鋼製造證書","issuedBy":{"@type":"Organization","name":"American Bureau of Shipping"},"validFrom":"2024-04-17"},{"@type":"Certification","name":"FPC 證書 EN 1090-1","issuedBy":{"@type":"Organization","name":"TUV Rheinland"},"validFrom":"2024-06-24"}]},{"@type":"WebSite","@id":"https://zh-hant.pipemanufactory.com/#website","name":"Gangyou Steel Manufacture Company","url":"https://zh-hant.pipemanufactory.com","publisher":{"@id":"https://pipemanufactory.com/#organization"},"inLanguage":"zh-Hant","potentialAction":{"@type":"SearchAction","target":{"@type":"EntryPoint","urlTemplate":"https://zh-hant.pipemanufactory.com/products?q={search_term_string}"},"query-input":"required name=search_term_string"}}]}
{"@context":"https://schema.org","@graph":[{"@type":"ItemPage","@id":"https://zh-hant.pipemanufactory.com/products/pipe-fittings/carbon-steel-flange/astm-a182-f22-alloy-steel-flanges#webpage","url":"https://zh-hant.pipemanufactory.com/products/pipe-fittings/carbon-steel-flange/astm-a182-f22-alloy-steel-flanges","name":"ASTM A182 F22 合金鋼法蘭 | 2.25Cr-1Mo 鉻鉬鋼 - Gangyou Steel","description":"符合 ASME B16.5/B16.47 標準的 2.25Cr-1Mo (UNS K21590) 材質的 ASTM A182 F22 法蘭，1 級和 3 級。請確認尺寸、等級和密封面以取得報價。","isPartOf":{"@id":"https://zh-hant.pipemanufactory.com/#website"},"inLanguage":"zh-Hant","primaryImageOfPage":{"@type":"ImageObject","url":"https://zh-hant.pipemanufactory.com/uploads/images/astm-a182-f347-flange-4.webp"},"breadcrumb":{"@id":"https://zh-hant.pipemanufactory.com/products/pipe-fittings/carbon-steel-flange/astm-a182-f22-alloy-steel-flanges#breadcrumb"},"mainEntity":{"@id":"https://zh-hant.pipemanufactory.com/products/pipe-fittings/carbon-steel-flange/astm-a182-f22-alloy-steel-flanges#product"}},{"@type":"BreadcrumbList","@id":"https://zh-hant.pipemanufactory.com/products/pipe-fittings/carbon-steel-flange/astm-a182-f22-alloy-steel-flanges#breadcrumb","itemListElement":[{"@type":"ListItem","position":1,"name":"首頁","item":"https://zh-hant.pipemanufactory.com/"},{"@type":"ListItem","position":2,"name":"產品","item":"https://zh-hant.pipemanufactory.com/products"},{"@type":"ListItem","position":3,"name":"管件","item":"https://zh-hant.pipemanufactory.com/products/pipe-fittings"},{"@type":"ListItem","position":4,"name":"碳鋼法蘭","item":"https://zh-hant.pipemanufactory.com/products/pipe-fittings/carbon-steel-flange"},{"@type":"ListItem","position":5,"name":"ASTM A182 F22 合金鋼法蘭","item":"https://zh-hant.pipemanufactory.com/products/pipe-fittings/carbon-steel-flange/astm-a182-f22-alloy-steel-flanges"}]},{"@type":"Product","@id":"https://zh-hant.pipemanufactory.com/products/pipe-fittings/carbon-steel-flange/astm-a182-f22-alloy-steel-flanges#product","name":"ASTM A182 F22 合金鋼法蘭","url":"https://zh-hant.pipemanufactory.com/products/pipe-fittings/carbon-steel-flange/astm-a182-f22-alloy-steel-flanges","mainEntityOfPage":{"@id":"https://zh-hant.pipemanufactory.com/products/pipe-fittings/carbon-steel-flange/astm-a182-f22-alloy-steel-flanges#webpage"},"brand":{"@type":"Brand","name":"Gangyou Steel"},"manufacturer":{"@id":"https://pipemanufactory.com/#organization"},"category":"管件 > 碳鋼法蘭","description":"產品說明 ASTM A182 F22 是一種鍛造 2.25Cr-1Mo（2&frac14; 鉻、1 鉬）低合金鋼級，用於高溫高壓工況下的管法蘭、鍛造管件及閥門零件。依此鋼種訂購的法蘭標示為 UNS K21590 及歐洲標號 W.Nr. 1.7380 (10CrMo9-10)；ASME SA-182 F22 則是該材料在鍋爐與壓力容器規範中的對應規格。 該鋼種通常以 3 級、正火及回火處理 狀態供應，此為管路及壓力部件的預設狀態。若需較低硬度或用於成形應用，可應要求提供 Class 1，退火處理 規格。法蘭尺寸、鑽孔規格及壓力等級並非由 A182 規範所規定，而是依據 ASME B16.5、ASME B16.47 或訂單中指定的圖面而定。 F22 在蠕變強度方面優於 F11（1.25Cr-0.5Mo），在抗高溫氫侵蝕能力方面則優於碳鋼，因此它是傳統發電廠主蒸汽管線和熱再熱管線，以及氫處理器、加氫裂解器與合成迴路法蘭接頭的標準選擇。此為低合金鋼，而非不鏽鋼，且並非因抗水腐蝕性而選用。請於詢價時確認適用規範、等級、表面處理及熱處理要求。 化學成分與產品形式 下表列出 F22 級別的 ASTM A182 / ASME SA-182 熔煉分析限值。此範圍同樣適用於 1 級和 3 級，兩者僅在熱處理及由此衍生的驗收值上有所不同。 元素 ASTM A182 F22 (%) 碳，C 0.05 – 0.15 錳，Mn 0.30 – 0.60 磷，P 最大 0.040 硫，S 最大 0.040 矽，Si 最大 0.50 鉻，Cr 2.00 – 2.50 鉬，Mo 0.87 – 1.13 鐵，Fe 餘量 在詢價階段有兩點需特別留意。ASTM A336 F22 規範涵蓋鍋爐及壓力容器鍛件所用的相同合金，但將磷與硫的含量分別限制在最高 0.025%，並要求進行夏比 V 型缺口衝擊試驗， 因此應明確指明適用規範，而非自行假設。此外， F22V （2.25Cr-1Mo-0.25V）為獨立鋼級，專為厚壁氫處理設備而刻意添加釩；其不可與普通 F22 互換使用。 F22 第 1 級與第 3 級的機械性能 F22 提供兩種熱處理狀態，且必須在詢價時明確標示等級，因為其驗收值有所不同。下表為 ASTM A182 規範中室溫下的要求值。 性質 第 1 級（退火） 第 3 級（正火及回火） 抗拉強度，最小值 415 MPa (60 ksi) 515 MPa (75 ksi) 屈服強度，最小值 205 MPa (30 ksi) 310 MPa (45 ksi) 50 mm 伸長率，最小 20% 20% 截面積減少率，最小 35% 30% 硬度 最大 170 HBW 156 – 207 HBW 典型用途 焊接堆焊母材、成形 管路及壓力部件（預設） ASTM A182 僅針對 F22 列出 1 級與 3 級規格。2 級規格僅適用於 F11 及 F12，不適用於 F22；若詢價時引用「F22 2 級」，應在放行鍛件前重新說明。根據 A182 規範，衝擊試驗並非強制性要求；若低溫韌性至關重要，則應在訂單中列為補充要求。針對酸性介質服務，NACE MR0175 / ISO 15156 規定此等級的硬度上限為 22 HRC，此限制必須納入熱處理週期中，而非事後進行檢測。 在 450 &deg;C 以上，設計應以蠕變為考量，而非室溫屈服強度。允許應力應參照 ASME BPVC 第 II 卷 D 部分，而非上文的驗收表。 法蘭類型、尺寸與壓力等級 F22 可鍛造為 B16.5 標準中的所有法蘭類型。下表彙總了尺寸標準所公布的內容；實際所需的法蘭類型、尺寸與等級，則由專案的管線等級決定。 項目 適用範圍 材料標準 ASTM A182 / ASME SA182，F22 級 (UNS K21590) 法蘭類型 焊接頸式、套接式、盲板式、承插焊式、螺紋式、搭接式、長焊接頸式、孔板式、縮徑式、眼鏡式盲板 尺寸，ASME B16.5 NPS 1/2 至 NPS 24 (DN 15 至 DN 600) 尺寸，ASME B16.47 NPS 26 至 NPS 60（DN 650 至 DN 1500），A 系列與 B 系列 壓力等級 ASME B16.5 150、300、400、600、900、1500、2500 級；ASME B16.47 各系列對應等級 端面型式 凸面（RF）、環形接頭（RTJ）、平面（FF） 焊接端面處理 對接焊端面符合 ASME B16.25 規範；管孔直徑與管徑規格相符 孔板法蘭 ASME B16.36，採用 B16.5 尺寸 認證 EN 10204 3.1 或 3.2 廠方測試證書；可應要求提供材料成分分析（PMI）及硬度檢測報告 B16.5 與 B16.47 屬於各自獨立的尺寸系列，而非同一份型錄；相同尺寸與等級的 A 系列與 B 系列通常無法相互螺栓連接——必須明確標示所屬系列。名義尺寸相符亦不能證明可相互配合：外徑、螺栓圓、孔數與孔徑、厚度、法蘭芯、內徑及端面均須與配對組件一致。 壓力等級的實際含義 常見將「Class 2500」解讀為「2500 psi」。該等級數值為無量綱的評級指標，並非壓力值。根據 ASME B16.5 標準，各級別的最大允許非衝擊工作壓力需參照法蘭材料組的壓力-溫度表查閱，且該數值會隨設計溫度升高而降低。F22 鍛件列於 B16.5 材料組 1.10 中，與 A217 WC9 鑄件及 A387 22 級鋼板同屬此組，該組的評級表適用範圍延伸至 1200 °F (650 °C)，其中 Class 150 的上限為 1000 ° F（538 °C）。 由此衍生出兩項後果。在 ASME B16.5 標準中，Class 2500 僅公布至 NPS 12 為止——較大尺寸則轉由 ASME B16.47 規範。此外，接合處的極限壓力可能由相連的管線、閥門、墊片或螺栓連接決定，而非由法蘭本身決定。請指定等級（而非 psi 數值），並參閱標準現行版本中關於設計溫度與壓制溫度的評定值。 F22 與 F11、F91 及 F22V 的比較 F22 是鉻鉬鋼系列中的其中一級。下表展示其在該系列中的定位；此表並非允許應力的來源，允許應力應參照設計規範。 鍛造等級 名義成分 適用範圍 F11 1.25Cr-0.5Mo 約 593 °C 以下的熱工程及蒸汽管線，此處無需 F22 的額外蠕變強度 F22 2.25Cr-1Mo 主蒸汽管線、熱再熱管線、氫處理及合成迴路 —— 本頁所列鋼級 F22V 2.25Cr-1Mo-0.25V 厚壁加氫處理反應器及封閉鍛件 F5 5Cr-0.5Mo 存在硫化物腐蝕的高鉻煉油應用 F9 9Cr-1Mo 煉油廠高溫侵蝕工況 F91 9Cr-1Mo-V-Nb 超臨界蒸汽；具有較高的蠕變強度，但焊接與熱處理要求更嚴格 比較已發佈的表格時，請留意 UNS 標號。第三方彙編資料常會將相同化學成分的管材（A335 P 系列）與鍛件（A182 F 系列）編號混為一談，且有多份網路表格會將管材編號與鍛件等級對應。若 UNS 標號在合約中至關重要，請以採購訂單上指定的版本為準，而非參考頁面上的資訊。 高溫蒸汽、氫氣工況及腐蝕極限 有兩種工況決定了 F22 的規格，而關於該等級的一項常見誤解值得在開頭就予以糾正。 高溫蒸汽。 由於鉬含量達全百分比，F22 的蠕變強度明顯高於 F11。在傳統化石燃料發電廠中，它是主蒸汽管、熱再熱集管、熱鍋爐連接管及渦輪引管之標準材料，適用溫度範圍最高可達 550–595 °C；此為選材範圍，而非額定值。在 450 °C 以上，設計主要由蠕變強度而非屈服強度決定，因此允許應力應參照 ASME BPVC 第 II 卷 D 部分或適用之設計規範，而非本頁所列之驗收值。 耐高溫氫侵蝕性。 在高溫及高氫分壓條件下，鋼中的碳會與氫反應生成甲烷，由於甲烷無法從金屬中擴散出去，將導致內部龜裂及起泡。F22 中 2.25% 的鉻含量可鎖住碳元素，並提高此現象構成風險所需的溫度與氫分壓。允許的組合由 API 941 中的 Nelson 曲線標示，其中 2.25Cr-1Mo 的位置高於碳鋼及 1.25Cr-0.5Mo。正因如此，氫處理器與加氫裂解反應器迴路、氨與甲醇合成迴路，以及氫氣回收壓縮機管路，通常會將 F22 法蘭與 A335 P22 管材及 A234 WP22 管件指定為配套組合。 F22 並非什麼材料。 F22 的鉻含量為 2.25%，屬於低合金鋼——遠低於形成鈍化表面膜所需的 10.5% 鉻含量。它並非不鏽鋼，對水介質腐蝕毫無實質抵抗力：在環境濕式工況下，其生鏽程度與碳鋼無異。其合金成分旨在提升高溫下的蠕變強度和抗氫性能，而非抗腐蝕性。若需對抗濕式腐蝕，應選用 300 系列或雙相不鏽鋼等級；針對高溫硫化物煉油流體，則應選用鉻含量更高的 F5 和 F9 等級。 熱處理、焊接與焊後熱處理 F22 確實具有空氣淬火特性：焊縫的熱影響區在靜止空氣中會自行淬硬，因此製造過程必須事先規劃，而非即興應變。每件 F22 鍛件均經過熱處理，法蘭即以該狀態供應。典型製造要求摘要如下。 項目 典型要求 鍛件的熱處理 正火與回火，或淬火與回火； 至少在 675 °C (1250 °F) 進行 3 級回火 焊接前預熱 通常為 200–300 °C (392–572 °F) 耗材 適用於 2.25Cr-1Mo 的焊材：E9018-B3（SMAW）、ER90S-B3（GTAW / GMAW） 焊後熱處理 2.25Cr 級別必須進行 — 通常為 690–750 °C (1275–1380 °F) 焊後熱處理溫度限制 必須低於母材鍛件所施行的回火溫度 實務要點 低氫耗材、受控的道間溫度、熔爐編號的完整可追溯性 其中兩項應從一開始就列入採購訂單。根據 ASME B31.1 及 B31.3 規範，2.25Cr 級材料在幾乎所有實際厚度下均需進行焊後熱處理，因此必須納入施工規範，而非事後追加。此外，焊後熱處理（PWHT）的溫度必須低於母材鍛件所使用的回火溫度：即使法蘭本身在離開鍛造廠時符合規格，接頭處的過度回火仍會破壞法蘭的認證機械性能。 若管線等級允許使用套接法蘭，其成本較低且安裝更為簡便；但在蠕變範圍及週期性工況下，通常僅限採用焊頸式設計，因其全熔透對接焊可進行射線檢測，且抗熱疲勞性能優於角焊縫。 針對厚壁或長壽命高溫工況，訂單中可能還會包含回火脆化控制措施——包括焊縫金屬的 J 因子限值與 Bruscato X-bar 限值——並需進行階梯式冷卻及夏比衝擊試驗。這些屬於補充要求：它們不屬於 A182 基礎標準的一部分，必須在詢價時明確說明。 ASTM A182 F22 法蘭的應用 典型應用包括： 傳統及 HRSG 發電廠中的主蒸汽與熱再熱集管、熱鍋爐連接件及渦輪引管。 加氫處理器、加氫裂解器及重整反應器迴路，以及氫氣回收壓縮機管路，此處法蘭接頭必須符合 API 941 奈爾森曲線規範。 氨與甲醇合成迴路，以及高壓分離器與熱閃蒸鼓的接管連接處。 煉油廠與石化廠的高溫工藝管路，通常作為搭配 A335 P22 管材及 A234 WP22 管件的 2.25Cr-1Mo 系統的一部分。 設計溫度、氫氣分壓以及任何含硫工況要求，是決定是否僅需普通 F22 鋼級，抑或需採用 F22V 或 9Cr 鋼級的三大考量因素。在確定鋼級與熱處理方式前，請先確認這些參數。 訂購資訊 如需報價 ASTM A182 F22 法蘭，需提供以下資訊： 鋼級與等級 —— ASTM A182 F22 1 級或 3 級。3 級為預設選項；F22 並無 2 級規格。 法蘭類型與端面 —— 焊接頸、套接式、盲板、承插焊、螺紋、搭接式、長焊接頸或孔口；RF、RTJ 或 FF。 尺寸與壓力等級 —— 公稱尺寸及對應的尺寸標準：ASME B16.5、ASME B16.47 A 系列或 B 系列、ASME B16.36，或相關圖紙。 內徑或管壁厚度等級 —— 焊接頸部及長焊接頸部類型必須指定此項，以確保內徑與配","image":["https://zh-hant.pipemanufactory.com/uploads/images/astm-a182-f347-flange-4.webp","https://zh-hant.pipemanufactory.com/uploads/images/astm-a182-f22-alloy-steel-flanges-1.webp","https://zh-hant.pipemanufactory.com/uploads/images/astm-a182-f22-alloy-steel-flanges-3.webp","https://zh-hant.pipemanufactory.com/uploads/images/astm-a182-f22-alloy-steel-flanges-4.webp"],"sku":"HJGFL001","additionalProperty":[{"@type":"PropertyValue","name":"材料","value":"ASTM A182 F22 (2.25Cr-1Mo), UNS K21590, W.Nr. 1.7380"},{"@type":"PropertyValue","name":"級別","value":"3 級標準化並調質；1 級可按要求退火"},{"@type":"PropertyValue","name":"法蘭類型","value":"焊頸、套焊、盲板、承插焊、螺紋、重疊接頭、長焊頸、孔板"},{"@type":"PropertyValue","name":"尺寸範圍","value":"NPS 1/2-24 對應 ASME B16.5；NPS 26-60 對應 ASME B16.47 系列 A/B"},{"@type":"PropertyValue","name":"壓力等級","value":"150-2500等級（ASME B16.5，2500等級至NPS 12）；按系列的B16.47等級"},{"@type":"PropertyValue","name":"密封面","value":"凸面法蘭 (RF)、環型接頭法蘭 (RTJ)、平面法蘭 (FF)"}]}]}
```