title: 12.9 六角螺栓 | ISO 898-1 淬火及回火合金鋼 - Gangyou Steel
description: 12.9 級六角螺栓，合金鋼材質，符合 ISO 898-1 標準，經淬火及回火處理，最小抗拉強度為 1220 MPa。請確認直徑、螺紋和塗層要求以取得報價。
image: https://zh-hant.pipemanufactory.com/uploads/images/129-hex-bolt-1.webp
---

![12.9 六角螺栓](/uploads/images/129-hex-bolt-1.webp)

# 12.9 六角螺栓

12.9 級六角螺栓，合金鋼材質，依 ISO 898-1 進行淬火與回火，最低抗拉強度 1,220 MPa，硬度範圍 385 - 435 HV。請確認直徑、螺紋範圍及塗層以便報價。

**強度等級**

12.9 依 ISO 898-1

**材料**

合金鋼，淬火回火，最低回火溫度425°C（SCM435、35CrMo、42CrMo4）；或加合金元素的碳鋼，淬火回火，最低回火溫度380°C

**最小抗拉強度**

1,220 兆帕（名義上 1,200 兆帕）

**最小 0.2% 屈服應力**

1,100 兆帕（名義上 1,080 兆帕）

**硬度**

385 - 435 HV / 380 - 429 HBW / 39 - 44 HRC

**尺寸、螺紋與表面處理**

直徑、螺距及螺紋範圍符合 ISO 4014 或 ISO 4017；表面處理可為普通、黑色氧化、鋅鎳或鋅片，依訂單確認

[發送詢價](/inquiry?products=1507) [WhatsApp](https://wa.me/8615875546993)

## 符合 ISO 898-1 標準的 12.9 級六角螺栓

12.9 級六角螺栓是常用公制系統中性能等級最高的螺栓：這是一種合金鋼製六角頭螺栓，經全截面淬火與回火處理，其最低抗拉強度為 1,220 MPa。此等級由 ISO 898-1 規範定義，該標準是針對螺栓、螺絲及螺柱機械性能的國際標準。「12.9 六角螺栓」與「12.9 級六角螺栓」均指同一種緊固件；ISO 稱之為「性能等級」，而北美買家通常稱之為「等級」。

此標示方式基於算術計算，並非行銷級別。第一個數字乘以 100 即得公稱抗拉強度（單位：MPa），因此 12 代表 1,200 MPa。小數點後的數字是公稱屈服強度與公稱抗拉強度的比值乘以十，因此 .9 表示公稱 0.2% 證明應力為公稱抗拉強度的 90%，即 1,080 MPa。該等級中的其他所有要求皆由這兩個數字推導而出：材料必須是合金鋼，必須經過整體淬火，且成品螺栓必須具備足夠的硬度和潔淨度，才能達到這些數值而不致變脆。

最後這一點正是 12.9 級螺栓與目錄中其他產品區別所在。10.9 級以下的螺栓是根據強度和價格選購的；而 12.9 級螺栓則需兼顧強度和製程控制，因為能提供 1,220 MPa 強度的同一種微觀組織，也會使該緊固件對氫氣以及回火後施加的任何熱量變得敏感。本頁闡述了性能等級的要求、材料與熱處理流程、決定螺栓頭部與螺紋尺寸的標準、在此強度等級下可安全施加的塗層，以及買方對進貨批次可進行的檢驗項目。

## 12.9 性能等級的要求

以下數值為 ISO 898-1 標準中針對 12.9 性能等級的要求，係在該標準適用於所有性能等級的 10°C 至 35°C 環境測試範圍內進行評估。由於供應商表格中常將「標稱值」與「最低值」混為一談，因此此處將兩者分開列出：標稱值是用於確定等級分類，而最低值則是測試證書必須達到的數值。

| | |
| --- | --- |
| 性能等級 | 12.9（依據 ISO 898-1） |
| 抗拉強度，公稱值 | 1,200 MPa |
| 抗拉強度，最低值 | 1,220 MPa |
| 0.2% 非比例伸長率下的應力，標稱值 | 1,080 MPa |
| 0.2% 非比例伸長率下的應力，最低值 | 1,100 MPa |
| 抗壓載荷下的應力，公稱值 | 970 MPa，抗壓強度比 0.88 |
| 斷後伸長率，最小值 | 8 百分比 |
| 截面積減少率，最小值 | 44 百分比 |
| 硬度 | 385 - 435 HV / 380 - 429 HBW / 39 - 44 HRC |
| 表面硬度，最大值 | 435 HV 0.3 |
| 材料 | 淬火回火合金鋼，最低回火溫度 425 C；或添加元素（硼、錳、鉻或鉬）的碳鋼，經淬火回火處理，最低回火溫度 380 C |
| 頭部標記 | 「12.9」搭配製造商識別標記 |

該表格中有四項細節值得特別留意，因為每一項都是導致批次被拒或報價爭議的常見原因。

首先是公稱抗拉強度與最低抗拉強度之間的差距。12.9級螺栓常被描述為「1,200 MPa」，這是該標稱系統所採用的公稱值；而試驗樣品實際必須達到的要求則是1,220 MPa。同樣的差異也適用於 0.2% 屈服應力：1,080 MPa 為公稱值，1,100 MPa 則為最低值。

第二點是證明載荷。12.9級螺栓在證明載荷下的名義應力為970 MPa，而非1,100 MPa。廣為流傳的1,100 MPa這個數字，被稱為「12.9級證明載荷」，實為最低0.2%證明應力，這是一個以不同方式測量的不同數值。標準中 0.88 的證明強度比，是根據 970 MPa 除以 1,100 MPa 的最低值計算得出的。

第三點是硬度範圍，這是一個雙向標準。測試硬度超過 435 HV 的螺栓屬於過度淬火，其脆性已超出該等級的允許範圍；而硬度低於 385 HV 的螺栓則無法達到拉伸強度的要求。位於硬度範圍中段的數值，是淬火與回火循環過程受控的機械證據。

第四項是直徑範圍。性能等級表適用於 M1.6 至 M39 的粗牙螺紋，以及 M8x1 至 M39x3 的細牙螺紋。超過 M39 時，雖仍可使用該等級標示，但僅限於緊固件符合該等級的所有要求，且尺寸經買方與製造商雙方同意的情況下——因此，「12.9 至 M100」的報價實為特殊訂製產品的聲明，而非標準等級。

## 12.9 級與 8.8 級及 10.9 級之比較

在詢價時，這三種高強度等級常被近乎互換地引用，但它們屬於不同材質，具有不同的延展性及不同的處理要求，且在接合處不可互換使用。以下比較採用 ISO 898-1 的最低值，因為接合處的設計是基於最低值，而非用於等級名稱的名義數值。

| | |
| --- | --- |
| 最低抗拉強度 | 8.8：800 MPa；10.9：1,040 MPa；12.9：1,220 MPa |
| 0.2% 非比例伸長率下的最低應力 | 8.8：640 MPa； 10.9：940 MPa；12.9：1,100 MPa |
| 斷後最小伸長率 | 8.8：12%；10.9：9%；12.9：8% |
| 硬度範圍 | 8.8：250 - 320 HV；10.9：320 - 380 HV；12.9：385 - 435 HV |
| 材料製程 | 8.8：添加元素的碳鋼、碳鋼或合金鋼； 10.9：上述三種製程；12.9：合金鋼，最低淬火溫度 425 C；或添加元素的碳鋼，最低淬火溫度 380 C |
| 氫脆敏感性 | 8.8 級較低，10.9 級較高，12.9 級極高 |
| 典型用途 | 8.8：一般工程與建築；10.9：汽車與重型機械；12.9：無法使用較大螺栓的緊湊型高負載接合處 |

該表格中有兩項數據常被錯誤引用。10.9 級的最低抗拉強度為 1,040 MPa，其最低 0.2% 證明應力為 940 MPa；那些將 10.9 級的數值標示為 1,000 MPa 和 900 MPa 的對照表，是將名義標稱值誤認為技術要求。12.9級同樣沒有英制等效規格：SAE 8級約為150 ksi，相當於1,034 MPa，低於12.9級的最低標準，因此英制專案若需12.9級強度，通常必須改用公制緊固件或特殊合金，而非以8級螺栓替代。

## 材料與熱處理

在本文採用的 ISO 898-1:2013 轉錄版本中，12.9 級有兩種製程。一種是合金鋼，經淬火與回火處理，最低回火溫度為 425 C，碳含量為 0.30 至 0.50 百分比。另一種則是添加了硼、錳、鉻或鉬等元素的碳鋼，經淬火與回火處理，最低回火溫度為 380 攝氏度，碳含量為 0.28% 至 0.50%。8.8 級和 10.9 級螺栓可由添加元素的碳鋼、普通碳鋼或合金鋼製成。以下限值適用於合金鋼製程。供應商不得僅對中碳螺栓進行淬火處理後，便將其標記為 12.9 級。

| | |
| --- | --- |
| 碳 (C) | 0.30 - 0.50 百分比 |
| 磷 (P) | 最高 0.025 百分比 |
| 硫 (S) | 最高 0.025 百分比 |
| 硼 (B) | 最高 0.003 百分比 |
| 鉻 (Cr) | 最低 0.30 百分比 — 四種合金元素中至少須含有一種 |
| 鎳 (Ni) | 0.30 百分比 最低 |
| 鉬 (Mo) | 0.20 百分比 最低 |
| 釩 (V) | 0.10 百分比 最低 |
| 最低回火溫度，合金鋼製程 | 425 C |
| 含添加劑之碳鋼，碳含量 | 0.28 - 0.50 百分比 |
| 最低回火溫度，含添加劑之碳鋼 | 380 C |

此表格附有三項說明。當兩種、三種或四種合金元素結合時，其總含量必須至少達到各元素最低含量總和的 70%——因此，鋼材若僅含有數種含量均未達標的微量元素，則無法滿足合金要求。在合金鋼製程中，回火下限為 425 C；在添加元素的碳鋼製程中，則為 380 C。每種下限均對應其特定製程：若螺栓的回火溫度低於所訂製程的下限，雖能通過硬度檢測，卻將無法滿足延展性要求。此外，12.9級還有一項額外的冶金限制：不允許存在經金相學可檢測到的白色磷化物層；由於該層必須在熱處理前去除，因此無法在成品螺栓上進行修正。

在商業實踐中，此等級的螺栓通常採用鉻鉬合金鋼製造。符合 JIS G4105 標準的 SCM435 是最廣泛使用的鋼種，大致對應於 35CrMo 和 AISI 4135；當該系列中較大直徑的螺栓需要額外的淬透性時，則使用 42CrMo 和 42CrMo4。淬透性會隨直徑增大而降低，因此鋼種通常會與尺寸一併指定，而非針對整個系列固定不變。當根據本頁內容核對廠家證明書時，有三個關鍵欄位需注意：鋼種與熔爐編號、以 425°C 為下限的回火溫度，以及落在 385–435 HV 範圍內的硬度結果——僅顯示硬度的證明書無法證明已滿足回火要求。

## 頭部形狀、螺紋與尺寸

ISO 898-1 僅定義機械性能；對螺栓的形狀未作任何規定。尺寸來自另一項產品標準，兩者通常在圖紙上一併標示。對於六角頭螺栓，相關的兩項標準為 ISO 4014 和 ISO 4017，兩者均針對產品等級 A 和 B 的 M1.6 至 M64 規格制定。

| | |
| --- | --- |
| ISO 4014 | 六角頭螺栓——具有定義明確的無螺紋軸桿，因此在尺寸和長度允許的情況下，螺紋為部分螺紋 |
| ISO 4017 | 六角頭螺釘——沿有效長度全長帶有螺紋，為全螺紋型號 |
| 產品等級 A 或 B | A 適用於螺紋直徑不超過 M24 且長度不超過 10d 或 150 mm（以較短者為準）；B 則適用於超出上述限值的規格。產品等級屬於尺寸公差類別，與材料等級並非同一概念 |
| 性能等級適用範圍 | M1.6 至 M39 採用標準性能等級，其中包括 12.9；M39 以上則依協議而定 |
| 12.9 級可選的螺紋範圍 | 在性能等級表範圍內，可選部分螺紋（ISO 4014）或全螺紋（ISO 4017），以及粗牙或細牙 |
| 表面不連續性 | 螺栓、螺釘及螺柱一般適用 ISO 6157-1，而 12.9 性能等級則適用 ISO 6157-3 的特殊要求 |
| 頭部標記 | 性能等級及製造商識別標記，依 ISO 898-1 規定 |

目前流傳的兩項說法，在被應用於圖面之前需予以更正。ISO 4014 並非重型六角或結構用螺栓標準，亦非與 ISO 4017 構成一對標準中的「結構」部分：這兩項標準均採用相同的大系列六角平頭，差異僅在於螺紋長度的比例。若圖面要求在剪切平面上具有明確定義的無螺紋軸桿，則該軸桿應指定為 ISO 4014，而非更重型的螺帽。

另一項是德國標準編號。DIN 912（現為 ISO 4762）屬於內六角螺釘，其螺帽形狀與產品類型皆不同。六角頭螺栓屬於 DIN 931 和 DIN 933 標準，這兩者是 ISO 4014 和 ISO 4017 的前身。將 DIN 912 視為六角頭螺栓的等效規格，是一種尺寸錯誤，這種錯誤通常要等到零件送達時才會顯現。

## 鍍層與氫脆

在 1,220 MPa 強度下，母材本身不具備實用的耐大氣腐蝕性，而大多數 12.9 級螺栓的現場失效皆始於鍍層：在酸洗或電鍍線中吸附的氫氣，可能遷移至受應力作用的螺紋根部，並在接合處擰緊數小時或數天後，導致延遲性脆性斷裂。以下是 12.9 級六角螺栓通常引用的規格類別，以及各類別的具體要求。

| | |
| --- | --- |
| 未經處理 | 無塗層，通常僅輕微潤油。適用於受保護的室內機械；若接合處需要定義摩擦係數，仍應註明潤滑劑名稱 |
| 黑氧化處理 | 一種用於美觀及輕度室內防護的薄轉化塗層；此非屏障塗層，且不屬於緊固件鋅片標準 ISO 10683 的規範範圍 |
| 鋅鎳電鍍 | ASTM B841：第 1 級涵蓋 5% 至 12% 的鎳含量，最低厚度為 5、8 及 10 級，並適用鉻酸鹽轉化類型 A 至 E。由於屬電解製程，此強度等級需進行氫脆緩解處理（鍍層後處理參照 ASTM B850， B849 規範前處理） |
| 鋅片 | ISO 10683 非電解鋅片塗層系統。此塗層無需電解沉積步驟，且厚度足夠薄，不會影響螺紋配合，因此通常是高強度緊固件的首選 |
| 機械鍍鋅 | ASTM B695。當需要較厚犧牲層時，可選用此非電解替代方案 |
| 熱浸鍍鋅 | ISO 10684。一般不建議用於 12.9 級：該製程溫度接近螺栓的回火範圍，且鍍層製程存在氫致裂風險。若需富鋅鍍層，採用非電解系統是更安全的選擇 |

以下為四項實務要點。緩解烘烤雖屬塗層後之工廠作業慣例（而非 ISO 898-1 之規定限值），應於 190 至 230 攝氏度下進行數小時，並應於塗層完成後儘速開始，因為必須在接頭受力前將氫氣驅除。塗層前之酸洗處理，在 12.9 級及以上級別中受到限制。塗層應以等級、級別及轉化類型進行標示，而非僅標示裸厚範圍，因為「8–12 微米」不符合 ASTM B841 的等級結構，且會讓電鍍廠自行決定。此外，塗層會改變摩擦係數，因此若接合處有指定的預緊力，塗層與潤滑劑應與螺栓一併納入詢價範圍——它們決定了能達到該預緊力的扭力值。

關於塗層有一項禁令：12.9級螺栓絕不可進行焊接。超過回火溫度的焊接熱量會破壞淬火回火狀態，因此無論螺栓頭部標示為何，經焊接的12.9級螺栓便不再是12.9級螺栓。

## ISO 898-1 未涵蓋的項目：扭力、剪切力與溫度

ISO 898-1 明確列出其規範範圍，同時也同樣重要地闡明其未涵蓋的項目：可焊性、耐腐蝕性、抗剪應力能力、扭力與夾緊力表現，以及抗疲勞性均不在本標準範圍內。關於扭力與夾緊力的測試方法另有一份獨立文件， ISO 16047，且任何 ISO 898-1 的性能等級數值均不得作為扭力或剪切強度來引用。

這對詢價而言有三個影響。12.9級螺栓不得公布任何剪切強度，因此任何包含「920 MPa」等剪切數值的規格，皆引用了標準中未載明的內容——本頁面舊版中附帶的該數值已因故移除，且接合處的剪切能力應來自接合計算，而非等級表。其次，螺栓本身並不具備扭力表：擰緊扭力是根據目標預緊力、螺紋應力面積以及實際塗層與潤滑劑的摩擦係數推算而來，因此同一顆螺栓在乾擰與潤滑狀態下所需的扭力不同，且未標明摩擦條件的扭力表不能直接套用。第三，機械性能值是在 10°C 至 35°C 範圍內評估的。該標準註明，緊固件在高溫或低溫下可能無法維持這些性能，而標準中關於此主題的附錄僅具參考性質——僅提供高溫下強度降低的近似值，並非驗收要求。所謂「最高可工作至 300°C」的性能承諾，實則是將該附錄誤讀為正式的等級標示。

## 進貨批次檢驗

12.9 級是遭仿冒最頻繁的緊固件等級之一，因為該等級標記易於標示且難以辨識。以下檢驗項目可依據交貨文件及首件樣品進行。

首先檢查螺帽。ISO 898-1 規定，性能等級與製造商識別標記必須永久標示於螺帽上；M5 及以下規格的螺帽可採用時鐘面標記代替數字。若螺栓僅標示等級數字而無製造商標記，或標記疑似於熱處理後才施加，則僅憑外觀無法認定其為 12.9 級。顏色與表面處理無法證明等級，因為同一款螺栓可供應光面、黑色、鋅片鍍層或鋅鎳鍍層等不同表面處理。

接著是機械性能的驗證。硬度值落在 385–435 HV 範圍內（或 39–44 HRC），雖是車間快速檢測的依據，但僅憑此尚不足夠；因為即使螺栓硬度值在該範圍內，若回火處理不當，仍可能不符合韌性要求。基準檢測應為對機加工試樣進行拉伸試驗，以驗證其是否達到 1,220 MPa 的最低要求， 並需一併報告伸長率與截面縮減率，此外還須依照 ISO 6157-3 標準對 12.9 級螺栓進行表面缺陷檢測。請在證書上確認爐號、鋼材等級及回火溫度：這三項資料正是將硬度讀數轉化為製程受控之證據的關鍵。

## 12.9級六角螺栓的適用與不適用場合

該等級的設計初衷是讓小型緊固件承受高負荷，因此主要應用於空間與重量受限、但負荷要求極高的場合：引擎、變速箱及懸吊系統接頭；破碎機、壓機和挖掘機等重型機械；模具、沖壓模及機床；風力發電機與齒輪箱的內部連接；以及採礦與建築設備。

有兩項界限與應用場景同樣重要。歐洲的預緊結構鋼構受 EN 14399 組裝系統規範，而該系統是基於 8.8 級和 10.9 級材料等級建立的——12.9 級並非結構螺栓等級之一，因此 12.9 級六角螺栓不能替代結構螺栓組裝。其英制等效規格——ASTM A325（120 ksi）與 A490（150 ksi）——是各自獨立的規範，擁有專屬的尺寸、螺紋及標記，並非以其他名稱標示的公制 12.9 級。壓力邊界與管路螺栓連接通常採用螺柱與螺母的規格，例如 A193 規格搭配 A194 規格的螺母，並依據適用的管路或壓力設備規範進行選用；若在受規範管制的接合處提案使用 12.9 級螺栓，必須先查閱相關規範，因為材料等級並不能取代規範中的螺栓規格要求。

腐蝕是另一項限制因素。無論屬何種等級，基材本身均不具耐腐蝕性，且在 12.9 等級下，塗層選項比 8.8 等級更為有限。當環境條件而非載荷成為主導設計考量時，應變更材料等級——不鏽鋼及雙相不鏽鋼緊固件系列連結如下——而非僅針對高強度合金鋼螺栓升級塗層。

## 訂購資訊

要為 12.9 級六角螺栓取得精確報價，必須同時明確說明以下各項，因為每項內容都會影響價格或生產流程：材料等級與標準，即 12.9 級符合 ISO 898-1； 尺寸標準與產品等級，例如 ISO 4014 或 ISO 4017 及 A 級或 B 級；公稱直徑、螺距與長度，以及是否需要部分或全螺紋；若已指定，則需提供鋼材等級，例如 SCM435、35CrMo 或 42CrMo； 塗層規格應以等級、級別及鉻酸鹽類型標示，並附上氫脆緩解要求；若接頭已進行設計，則需說明摩擦條件或所需的預緊力；匹配螺母等級，即符合 ISO 898-2 的 12 級；文件套件，通常包含載明爐批號及回火溫度的廠方證明書，以及機械性能測試報告；以及數量。若涉及高溫工作環境或腐蝕性環境，請在詢價時註明——這將決定塗層方案，以及是否應改報其他材料等級。

## 關於 12.9 級六角螺栓的常見問題

### 如何解讀 12.9 級螺栓頭部的標記？1,200 MPa 與 1,220 MPa 是否相同？

螺栓頭部標有「12.9」的性能等級，以及製造商的識別標記；「class」與「grade」意指相同概念——前者為 ISO 術語，後者為北美術語。關於數值，1,200 MPa 是該標示系統所依據的名義值，而 1,220 MPa 則是拉伸試驗試樣必須達到的最低值。同樣的區分也適用於 0.2% 屈服應力（其中 1,080 MPa 為標稱值，1,100 MPa 為最低值），以及屈服載荷（在屈服載荷下的標稱應力為 970 MPa）。

### 12.9級六角螺栓可以進行熱浸鍍鋅處理嗎？

一般不建議這樣做。鍍鋅過程會施加接近淬火回火高強度螺栓回火溫度範圍的高溫，且涉及酸洗預處理步驟，這兩者皆可能使1,220 MPa的材料面臨氫脆風險。若需採用富鋅塗層，較安全的規範應採用非電解方式，例如符合 ISO 10683 標準的鋅片塗層系統，或符合 ASTM B695 標準的機械鍍鋅；若已明定並記錄氫脆緩解處理程序，則符合 ASTM B841 標準的電鍍鋅鎳塗層亦可接受。

### 12.9級螺栓能否用於預應力結構鋼構？

不能作為結構螺栓組件使用。歐洲 EN 14399 標準中針對預應力結構連接的系統，是基於 8.8 級和 10.9 級的性能分級定義的；而北美結構螺栓 A325 和 A490 則屬於獨立的 UNC 規格。公制 12.9 六角螺栓雖能承載設計中的高強度接合，但其並不屬於結構螺栓系統範疇，且接合設計必須依據專案實際採用的規範進行驗證。

### 12.9 六角螺栓應搭配何種螺母使用？

符合 ISO 898-2 規範之 12 級螺母。螺母等級是根據驗證載荷與螺栓等級相匹配的；若使用較低等級的螺母，可能在螺栓達到其承載能力之前便發生滑牙，這會導致高強度接合處的組裝強度低於螺栓等級所暗示的水平。此外，螺母的塗層也應與螺栓的塗層相匹配，以確保接合設計中假設的摩擦條件仍然有效。

### 報價 12.9 六角螺栓需要哪些資訊？

性能等級與標準、尺寸標準與產品等級、直徑、螺距及包含螺紋長度的總長度、若已指定則需提供鋼材等級、塗層的等級、類別及類型（含氫脆緩解要求）、若螺母包含在供貨範圍內則需提供螺母等級、若使用環境與溫度有特殊要求則需說明、所需文件套件，以及數量。同時說明尺寸標準與塗層規格，方能使螺栓以「產品」而非「尺寸」的形式進行報價。

## 相關碳鋼緊固件系列

此系列中的其他等級適用於不同需求。[低碳鋼六角螺栓](/products/fasteners/carbon-steel-fasteners/mild-steel-hex-bolt) 以及 [ASTM A307 碳鋼螺栓](/products/fasteners/carbon-steel-fasteners/astm-a307-carbon-steel-bolts) 適用於低、中強度碳鋼工程，在此類應用中，12.9 級將是過度且延展性較差的選擇；完整產品系列歸類於 [碳鋼緊固件](/products/fasteners/carbon-steel-fasteners) 之下。針對壓力及管線螺栓應用，[ASTM A193 B7M 雙端螺柱](/products/fasteners/alloy-steel-bolts/astm-a193-b7m-double-ended-stud) 通常是規範中援引的標準。當設計主要考量腐蝕而非載荷時，應調整材料等級而非塗層，此時 [雙相不鏽鋼螺栓](/products/fasteners/duplex-steel-fasteners/duplex-2205-stainless-steel-bolts) 便是另一種選擇方案。

## 您可能還喜歡

[看更多](/products)

![ASTM A193 B7M 雙頭螺柱](/uploads/images/astm-a193-b7m-double-ended-stud-1.webp)

### [ASTM A193 B7M 雙頭螺柱](/products/fasteners/alloy-steel-bolts/astm-a193-b7m-double-ended-stud)

**等級**

ASTM A193/A193M B7M

**產品形式**

雙頭螺柱；兩端螺紋及光軸按圖紙

![雙相2205不銹鋼螺栓](/uploads/images/duplex-steel-threaded-rod-10.webp)

### [雙相2205不銹鋼螺栓](/products/fasteners/duplex-steel-fasteners/duplex-2205-stainless-steel-bolts)

**產品**

2205 雙倍六角螺栓。一個訂單，一個 UNS 編號。

**等級**

UNS S31803 或 UNS S32205（EN 1.4462）。不是 S32750 或 S32760。

![ASTM A307 碳鋼螺栓](/uploads/images/129-hex-bolt-2.webp)

### [ASTM A307 碳鋼螺栓](/products/fasteners/carbon-steel-fasteners/astm-a307-carbon-steel-bolts)

**標準**

ASTM A307-21 - 碳鋼螺栓、螺柱和螺紋杆，只使用英寸-磅單位，最小拉伸強度 60 ksi；沒有 A307M 版本

**等級**

A級（通用型）和B級（鑄鐵法蘭接頭）；C級於2007年取消，現在稱為ASTM F1554 36級

![用於 ASTM A307 螺栓的螺帽 — ASTM A563 A 級](/uploads/images/astm-a307-nuts-2.webp)

### [用於 ASTM A307 螺栓的螺帽 — ASTM A563 A 級](/products/fasteners/carbon-steel-fasteners/nuts-for-astm-a307-bolts-astm-a563-grade-a)

**螺帽等級與型式**

ASTM A563/A563M A級，全六角或厚六角，依 ASTM A307-21 第 1.3 條規定

**配對緊固件**

ASTM A307 A級和B級螺栓、螺柱和螺紋杆；A307 C級已撤銷，改由ASTM F1554 36級取代

```json
{"@context":"https://schema.org","@graph":[{"@type":"Organization","@id":"https://pipemanufactory.com/#organization","name":"Gangyou Steel Manufacture Company","alternateName":"Gangyou Steel","url":"https://pipemanufactory.com","logo":"https://pipemanufactory.com/uploads/images/ecfa6bb3-faec-48b0-8daa-81c94219bdaa.png","description":"Gangyou Steel supplies steel pipe, plate, coil, flanges, pipe fittings, fasteners, structural sections, round bar and industrial valves in carbon, stainless and alloy steel, from Foshan, China.","telephone":"+86-15875546993","email":"info@pipemanufactory.com","address":{"@type":"PostalAddress","streetAddress":"Gangtieshijie D7Qu 401 Jiagongqu er Road","addressLocality":"Foshan","addressRegion":"Guangdong","postalCode":"528000","addressCountry":"CN"},"contactPoint":{"@type":"ContactPoint","telephone":"+86-15875546993","email":"info@pipemanufactory.com","contactType":"customer service","availableLanguage":["en","es","de","fr","it","nl","pt","th","ko","vi","ja","id","ru","tr","zh-Hant","ar","no","hmn"]},"sameAs":["https://www.facebook.com/jerry.he.7731","https://www.instagram.com/jerry.he.7731"],"knowsAbout":["https://en.wikipedia.org/wiki/Steel","https://en.wikipedia.org/wiki/Stainless_steel","https://en.wikipedia.org/wiki/Carbon_steel","https://en.wikipedia.org/wiki/Alloy_steel","https://en.wikipedia.org/wiki/Duplex_stainless_steel","https://en.wikipedia.org/wiki/Pipe_(fluid_conveyance)","https://en.wikipedia.org/wiki/Piping_and_plumbing_fitting","https://en.wikipedia.org/wiki/Flange","https://en.wikipedia.org/wiki/Fastener","https://en.wikipedia.org/wiki/Valve","https://en.wikipedia.org/wiki/Structural_steel","https://en.wikipedia.org/wiki/Sheet_metal","https://en.wikipedia.org/wiki/Galvanization"],"hasCertification":[{"@type":"Certification","name":"PED 2014/68/EU 指令","issuedBy":{"@type":"Organization","name":"TUV Rheinland"},"validFrom":"2024-03-29"},{"@type":"Certification","name":"ASME U-Stamp 認證","issuedBy":{"@type":"Organization","name":"The American Society of Mechanical Engineers"},"validFrom":"2023-11-14"},{"@type":"Certification","name":"NORSOK M-650 資格認證","issuedBy":{"@type":"Organization","name":"DNV GL"},"validFrom":"2024-07-07"},{"@type":"Certification","name":"ISO 3834-2 焊接認證","issuedBy":{"@type":"Organization","name":"TUV Nord"},"validFrom":"2024-08-11"},{"@type":"Certification","name":"Lloyd Register 類型批准","issuedBy":{"@type":"Organization","name":"Lloyd Register"},"validFrom":"2024-05-04"},{"@type":"Certification","name":"中國 CCC 認證","issuedBy":{"@type":"Organization","name":"CNCA"},"validFrom":"2024-08-31"},{"@type":"Certification","name":"ABS 鋼製造證書","issuedBy":{"@type":"Organization","name":"American Bureau of Shipping"},"validFrom":"2024-04-17"},{"@type":"Certification","name":"FPC 證書 EN 1090-1","issuedBy":{"@type":"Organization","name":"TUV Rheinland"},"validFrom":"2024-06-24"}]},{"@type":"WebSite","@id":"https://zh-hant.pipemanufactory.com/#website","name":"Gangyou Steel Manufacture Company","url":"https://zh-hant.pipemanufactory.com","publisher":{"@id":"https://pipemanufactory.com/#organization"},"inLanguage":"zh-Hant","potentialAction":{"@type":"SearchAction","target":{"@type":"EntryPoint","urlTemplate":"https://zh-hant.pipemanufactory.com/products?q={search_term_string}"},"query-input":"required name=search_term_string"}}]}
{"@context":"https://schema.org","@graph":[{"@type":"ItemPage","@id":"https://zh-hant.pipemanufactory.com/products/fasteners/alloy-steel-bolts/12-9-hex-bolt#webpage","url":"https://zh-hant.pipemanufactory.com/products/fasteners/alloy-steel-bolts/12-9-hex-bolt","name":"12.9 六角螺栓 | ISO 898-1 淬火及回火合金鋼 - Gangyou Steel","description":"12.9 級六角螺栓，合金鋼材質，符合 ISO 898-1 標準，經淬火及回火處理，最小抗拉強度為 1220 MPa。請確認直徑、螺紋和塗層要求以取得報價。","isPartOf":{"@id":"https://zh-hant.pipemanufactory.com/#website"},"inLanguage":"zh-Hant","primaryImageOfPage":{"@type":"ImageObject","url":"https://zh-hant.pipemanufactory.com/uploads/images/129-hex-bolt-1.webp"},"breadcrumb":{"@id":"https://zh-hant.pipemanufactory.com/products/fasteners/alloy-steel-bolts/12-9-hex-bolt#breadcrumb"},"mainEntity":{"@id":"https://zh-hant.pipemanufactory.com/products/fasteners/alloy-steel-bolts/12-9-hex-bolt#product"}},{"@type":"BreadcrumbList","@id":"https://zh-hant.pipemanufactory.com/products/fasteners/alloy-steel-bolts/12-9-hex-bolt#breadcrumb","itemListElement":[{"@type":"ListItem","position":1,"name":"首頁","item":"https://zh-hant.pipemanufactory.com/"},{"@type":"ListItem","position":2,"name":"產品","item":"https://zh-hant.pipemanufactory.com/products"},{"@type":"ListItem","position":3,"name":"緊固件","item":"https://zh-hant.pipemanufactory.com/products/fasteners"},{"@type":"ListItem","position":4,"name":"合金鋼螺栓","item":"https://zh-hant.pipemanufactory.com/products/fasteners/alloy-steel-bolts"},{"@type":"ListItem","position":5,"name":"12.9 六角螺栓","item":"https://zh-hant.pipemanufactory.com/products/fasteners/alloy-steel-bolts/12-9-hex-bolt"}]},{"@type":"Product","@id":"https://zh-hant.pipemanufactory.com/products/fasteners/alloy-steel-bolts/12-9-hex-bolt#product","name":"12.9 六角螺栓","url":"https://zh-hant.pipemanufactory.com/products/fasteners/alloy-steel-bolts/12-9-hex-bolt","mainEntityOfPage":{"@id":"https://zh-hant.pipemanufactory.com/products/fasteners/alloy-steel-bolts/12-9-hex-bolt#webpage"},"brand":{"@type":"Brand","name":"Gangyou Steel"},"manufacturer":{"@id":"https://pipemanufactory.com/#organization"},"category":"緊固件 > 合金鋼螺栓","description":"符合 ISO 898-1 標準的 12.9 級六角螺栓 12.9 級六角螺栓是常用公制系統中性能等級最高的螺栓：這是一種合金鋼製六角頭螺栓，經全截面淬火與回火處理，其最低抗拉強度為 1,220 MPa。此等級由 ISO 898-1 規範定義，該標準是針對螺栓、螺絲及螺柱機械性能的國際標準。「12.9 六角螺栓」與「12.9 級六角螺栓」均指同一種緊固件；ISO 稱之為「性能等級」，而北美買家通常稱之為「等級」。 此標示方式基於算術計算，並非行銷級別。第一個數字乘以 100 即得公稱抗拉強度（單位：MPa），因此 12 代表 1,200 MPa。小數點後的數字是公稱屈服強度與公稱抗拉強度的比值乘以十，因此 .9 表示公稱 0.2% 證明應力為公稱抗拉強度的 90%，即 1,080 MPa。該等級中的其他所有要求皆由這兩個數字推導而出：材料必須是合金鋼，必須經過整體淬火，且成品螺栓必須具備足夠的硬度和潔淨度，才能達到這些數值而不致變脆。 最後這一點正是 12.9 級螺栓與目錄中其他產品區別所在。10.9 級以下的螺栓是根據強度和價格選購的；而 12.9 級螺栓則需兼顧強度和製程控制，因為能提供 1,220 MPa 強度的同一種微觀組織，也會使該緊固件對氫氣以及回火後施加的任何熱量變得敏感。本頁闡述了性能等級的要求、材料與熱處理流程、決定螺栓頭部與螺紋尺寸的標準、在此強度等級下可安全施加的塗層，以及買方對進貨批次可進行的檢驗項目。 12.9 性能等級的要求 以下數值為 ISO 898-1 標準中針對 12.9 性能等級的要求，係在該標準適用於所有性能等級的 10°C 至 35°C 環境測試範圍內進行評估。由於供應商表格中常將「標稱值」與「最低值」混為一談，因此此處將兩者分開列出：標稱值是用於確定等級分類，而最低值則是測試證書必須達到的數值。 性能等級 12.9（依據 ISO 898-1） 抗拉強度，公稱值 1,200 MPa 抗拉強度，最低值 1,220 MPa 0.2% 非比例伸長率下的應力，標稱值 1,080 MPa 0.2% 非比例伸長率下的應力，最低值 1,100 MPa 抗壓載荷下的應力，公稱值 970 MPa，抗壓強度比 0.88 斷後伸長率，最小值 8 百分比 截面積減少率，最小值 44 百分比 硬度 385 - 435 HV / 380 - 429 HBW / 39 - 44 HRC 表面硬度，最大值 435 HV 0.3 材料 淬火回火合金鋼，最低回火溫度 425 C；或添加元素（硼、錳、鉻或鉬）的碳鋼，經淬火回火處理，最低回火溫度 380 C 頭部標記 「12.9」搭配製造商識別標記 該表格中有四項細節值得特別留意，因為每一項都是導致批次被拒或報價爭議的常見原因。 首先是公稱抗拉強度與最低抗拉強度之間的差距。12.9級螺栓常被描述為「1,200 MPa」，這是該標稱系統所採用的公稱值；而試驗樣品實際必須達到的要求則是1,220 MPa。同樣的差異也適用於 0.2% 屈服應力：1,080 MPa 為公稱值，1,100 MPa 則為最低值。 第二點是證明載荷。12.9級螺栓在證明載荷下的名義應力為970 MPa，而非1,100 MPa。廣為流傳的1,100 MPa這個數字，被稱為「12.9級證明載荷」，實為最低0.2%證明應力，這是一個以不同方式測量的不同數值。標準中 0.88 的證明強度比，是根據 970 MPa 除以 1,100 MPa 的最低值計算得出的。 第三點是硬度範圍，這是一個雙向標準。測試硬度超過 435 HV 的螺栓屬於過度淬火，其脆性已超出該等級的允許範圍；而硬度低於 385 HV 的螺栓則無法達到拉伸強度的要求。位於硬度範圍中段的數值，是淬火與回火循環過程受控的機械證據。 第四項是直徑範圍。性能等級表適用於 M1.6 至 M39 的粗牙螺紋，以及 M8x1 至 M39x3 的細牙螺紋。超過 M39 時，雖仍可使用該等級標示，但僅限於緊固件符合該等級的所有要求，且尺寸經買方與製造商雙方同意的情況下——因此，「12.9 至 M100」的報價實為特殊訂製產品的聲明，而非標準等級。 12.9 級與 8.8 級及 10.9 級之比較 在詢價時，這三種高強度等級常被近乎互換地引用，但它們屬於不同材質，具有不同的延展性及不同的處理要求，且在接合處不可互換使用。以下比較採用 ISO 898-1 的最低值，因為接合處的設計是基於最低值，而非用於等級名稱的名義數值。 最低抗拉強度 8.8：800 MPa；10.9：1,040 MPa；12.9：1,220 MPa 0.2% 非比例伸長率下的最低應力 8.8：640 MPa； 10.9：940 MPa；12.9：1,100 MPa 斷後最小伸長率 8.8：12%；10.9：9%；12.9：8% 硬度範圍 8.8：250 - 320 HV；10.9：320 - 380 HV；12.9：385 - 435 HV 材料製程 8.8：添加元素的碳鋼、碳鋼或合金鋼； 10.9：上述三種製程；12.9：合金鋼，最低淬火溫度 425 C；或添加元素的碳鋼，最低淬火溫度 380 C 氫脆敏感性 8.8 級較低，10.9 級較高，12.9 級極高 典型用途 8.8：一般工程與建築；10.9：汽車與重型機械；12.9：無法使用較大螺栓的緊湊型高負載接合處 該表格中有兩項數據常被錯誤引用。10.9 級的最低抗拉強度為 1,040 MPa，其最低 0.2% 證明應力為 940 MPa；那些將 10.9 級的數值標示為 1,000 MPa 和 900 MPa 的對照表，是將名義標稱值誤認為技術要求。12.9級同樣沒有英制等效規格：SAE 8級約為150 ksi，相當於1,034 MPa，低於12.9級的最低標準，因此英制專案若需12.9級強度，通常必須改用公制緊固件或特殊合金，而非以8級螺栓替代。 材料與熱處理 在本文採用的 ISO 898-1:2013 轉錄版本中，12.9 級有兩種製程。一種是合金鋼，經淬火與回火處理，最低回火溫度為 425 C，碳含量為 0.30 至 0.50 百分比。另一種則是添加了硼、錳、鉻或鉬等元素的碳鋼，經淬火與回火處理，最低回火溫度為 380 攝氏度，碳含量為 0.28% 至 0.50%。8.8 級和 10.9 級螺栓可由添加元素的碳鋼、普通碳鋼或合金鋼製成。以下限值適用於合金鋼製程。供應商不得僅對中碳螺栓進行淬火處理後，便將其標記為 12.9 級。 碳 (C) 0.30 - 0.50 百分比 磷 (P) 最高 0.025 百分比 硫 (S) 最高 0.025 百分比 硼 (B) 最高 0.003 百分比 鉻 (Cr) 最低 0.30 百分比 — 四種合金元素中至少須含有一種 鎳 (Ni) 0.30 百分比 最低 鉬 (Mo) 0.20 百分比 最低 釩 (V) 0.10 百分比 最低 最低回火溫度，合金鋼製程 425 C 含添加劑之碳鋼，碳含量 0.28 - 0.50 百分比 最低回火溫度，含添加劑之碳鋼 380 C 此表格附有三項說明。當兩種、三種或四種合金元素結合時，其總含量必須至少達到各元素最低含量總和的 70%——因此，鋼材若僅含有數種含量均未達標的微量元素，則無法滿足合金要求。在合金鋼製程中，回火下限為 425 C；在添加元素的碳鋼製程中，則為 380 C。每種下限均對應其特定製程：若螺栓的回火溫度低於所訂製程的下限，雖能通過硬度檢測，卻將無法滿足延展性要求。此外，12.9級還有一項額外的冶金限制：不允許存在經金相學可檢測到的白色磷化物層；由於該層必須在熱處理前去除，因此無法在成品螺栓上進行修正。 在商業實踐中，此等級的螺栓通常採用鉻鉬合金鋼製造。符合 JIS G4105 標準的 SCM435 是最廣泛使用的鋼種，大致對應於 35CrMo 和 AISI 4135；當該系列中較大直徑的螺栓需要額外的淬透性時，則使用 42CrMo 和 42CrMo4。淬透性會隨直徑增大而降低，因此鋼種通常會與尺寸一併指定，而非針對整個系列固定不變。當根據本頁內容核對廠家證明書時，有三個關鍵欄位需注意：鋼種與熔爐編號、以 425°C 為下限的回火溫度，以及落在 385–435 HV 範圍內的硬度結果——僅顯示硬度的證明書無法證明已滿足回火要求。 頭部形狀、螺紋與尺寸 ISO 898-1 僅定義機械性能；對螺栓的形狀未作任何規定。尺寸來自另一項產品標準，兩者通常在圖紙上一併標示。對於六角頭螺栓，相關的兩項標準為 ISO 4014 和 ISO 4017，兩者均針對產品等級 A 和 B 的 M1.6 至 M64 規格制定。 ISO 4014 六角頭螺栓——具有定義明確的無螺紋軸桿，因此在尺寸和長度允許的情況下，螺紋為部分螺紋 ISO 4017 六角頭螺釘——沿有效長度全長帶有螺紋，為全螺紋型號 產品等級 A 或 B A 適用於螺紋直徑不超過 M24 且長度不超過 10d 或 150 mm（以較短者為準）；B 則適用於超出上述限值的規格。產品等級屬於尺寸公差類別，與材料等級並非同一概念 性能等級適用範圍 M1.6 至 M39 採用標準性能等級，其中包括 12.9；M39 以上則依協議而定 12.9 級可選的螺紋範圍 在性能等級表範圍內，可選部分螺紋（ISO 4014）或全螺紋（ISO 4017），以及粗牙或細牙 表面不連續性 螺栓、螺釘及螺柱一般適用 ISO 6157-1，而 12.9 性能等級則適用 ISO 6157-3 的特殊要求 頭部標記 性能等級及製造商識別標記，依 ISO 898-1 規定 目前流傳的兩項說法，在被應用於圖面之前需予以更正。ISO 4014 並非重型六角或結構用螺栓標準，亦非與 ISO 4017 構成一對標準中的「結構」部分：這兩項標準均採用相同的大系列六角平頭，差異僅在於螺紋長度的比例。若圖面要求在剪切平面上具有明確定義的無螺紋軸桿，則該軸桿應指定為 ISO 4014，而非更重型的螺帽。 另一項是德國標準編號。DIN 912（現為 ISO 4762）屬於內六角螺釘，其螺帽形狀與產品類型皆不同。六角頭螺栓屬於 DIN 931 和 DIN 933 標準，這兩者是 ISO 4014 和 ISO 4017 的前身。將 DIN 912 視為六角頭螺栓的等效規格，是一種尺寸錯誤，這種錯誤通常要等到零件送達時才會顯現。 鍍層與氫脆 在 1,220 MPa 強度下，母材本身不具備實用的耐大氣腐蝕性，而大多數 12.9 級螺栓的現場失效皆始於鍍層：在酸洗或電鍍線中吸附的氫氣，可能遷移至受應力作用的螺紋根部，並在接合處擰緊數小時或數天後，導致延遲性脆性斷裂。以下是 12.9 級六角螺栓通常引用的規格類別，以及各類別的具體要求。 未經處理 無塗層，通常僅輕微潤油。適用於受保護的室內機械；若接合處需要定義摩擦係數，仍應註明潤滑劑名稱 黑氧化處理 一種用於美觀及輕度室內防護的薄轉化塗層；此非屏障塗層，且不屬於緊固件鋅片標準 ISO 10683 的規範範圍 鋅鎳電鍍 ASTM B841：第 1 級涵蓋 5% 至 12% 的鎳含量，最低厚度為 5、8 及 10 級，並適用鉻酸鹽轉化類型 A 至 E。由於屬電解製程，此強度等級需進行氫脆緩解處理（鍍層後處理參照 ASTM B850， B849 規範前處理） 鋅片 ISO 10683 非電解鋅片塗層系統。此塗層無需電解沉積步驟，且厚度足夠薄，不會影響螺紋配合，因此通常是高強度緊固件的首選 機械鍍鋅 ASTM B695。當需要較厚犧牲層時，可選用此非電解替代方案 熱浸鍍鋅 ISO 10684。一般不建議用於 12.9 級：該製程溫度接近螺栓的回火範圍，且鍍層製程存在氫致裂風險。若需富鋅鍍層，採用非電解系統是更安全的選擇 以下為四項實務要點。緩解烘烤雖屬塗層後之工廠作業慣例（而非 ISO 898-1 之規定限值），應於 190 至 230 攝氏度下進行數小時，並應於塗層完成後儘速開始，因為必須在接頭受力前將氫氣驅除。塗層前之","image":["https://zh-hant.pipemanufactory.com/uploads/images/129-hex-bolt-1.webp","https://zh-hant.pipemanufactory.com/uploads/images/129-hex-bolt-2.webp","https://zh-hant.pipemanufactory.com/uploads/images/129-hex-bolt-3.webp","https://zh-hant.pipemanufactory.com/uploads/images/129-hex-bolt-4.webp","https://zh-hant.pipemanufactory.com/uploads/images/129-hex-bolt-5.webp","https://zh-hant.pipemanufactory.com/uploads/images/129-hex-bolt-7.webp","https://zh-hant.pipemanufactory.com/uploads/images/129-hex-bolt-8.webp","https://zh-hant.pipemanufactory.com/uploads/images/129-hex-bolt-9.webp","https://zh-hant.pipemanufactory.com/uploads/images/carbon-steel-hex-nut-4.webp"],"sku":"LJLS001","additionalProperty":[{"@type":"PropertyValue","name":"強度等級","value":"12.9 依 ISO 898-1"},{"@type":"PropertyValue","name":"材料","value":"合金鋼，淬火回火，最低回火溫度425°C（SCM435、35CrMo、42CrMo4）；或加合金元素的碳鋼，淬火回火，最低回火溫度380°C"},{"@type":"PropertyValue","name":"最小抗拉強度","value":"1,220 兆帕（名義上 1,200 兆帕）"},{"@type":"PropertyValue","name":"最小 0.2% 屈服應力","value":"1,100 兆帕（名義上 1,080 兆帕）"},{"@type":"PropertyValue","name":"硬度","value":"385 - 435 HV / 380 - 429 HBW / 39 - 44 HRC"},{"@type":"PropertyValue","name":"尺寸、螺紋與表面處理","value":"直徑、螺距及螺紋範圍符合 ISO 4014 或 ISO 4017；表面處理可為普通、黑色氧化、鋅鎳或鋅片，依訂單確認"}]}]}
```